按目标密度选择粒径规格,下表为各牌号的典型发泡倍率(倍)。
| 规格 | 平均粒径 (mm) | FL | F | FM | FG | E | B | H |
|---|---|---|---|---|---|---|---|---|
| MS | 1.2 – 1.8 | 60–70 | 70–85 | 60–70 | 60–70 | 70–85 | 60–70 | 75–85 |
| SA | 0.9 – 1.4 | 50–60 | 60–70 | 50–60 | 50–60 | 60–70 | 50–60 | 65–75 |
| SB | 0.7 – 1.1 | 40–55 | 50–65 | 40–55 | 40–55 | 50–65 | 40–55 | 55–65 |
| S | 0.5 – 0.9 | 30–45 | 35–50 | 30–45 | 30–45 | 35–50 | 30–45 | 40–55 |
| 4S | 0.3 – 0.6 | 20–30 | 20–35 | 20–30 | 20–30 | 20–35 | 20–30 | 25–40 |
粒径越大可达到的倍率越高(密度越低);粒径越小,薄壁包装制品表面细节越好。
| 原料理化性能(典型值) | |
|---|---|
| 外观性状 | 半透明/乳白色圆形颗粒 |
| 粒径范围 | 0.25 – 2.5 mm |
| 相对密度 | 1.03 |
| 堆积密度 | 约 610 kg/m³ |
| 软化点 | 70 – 85 ℃ |
| 水分含量 | ≤ 0.5% |
| 残留苯乙烯 | ≤ 0.3% |
| 筛析效率 | ≥ 90%(QB/T 4009-2010) |